CAS No.: | 9002-88-4 |
---|---|
Formula: | (C2h4)N |
EINECS: | 618-339-3 |
Still deciding? Get samples of US$ 1/Bag
Request Sample
|
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
No. | Properties | Value (SI Units) | Method |
01 | Density | 0.946 g/cm3 | ASTM D1505 |
02 | Melt Index, Condition 190°C / 2.16 kg | 0.18 g/10 min | ASTM D1238 |
03 | Brittleness Temperature, Type A clamp, Type I specimen | <-75°C | ASTM D746 |
04 | ESCR, Condition B (100% Igepal), F50 | >1000 hrs | ASTM D1693 |
05 | Flexural Modulus, Tangent - 16:1 span:depth, 12.7 mm/min | 1150 MPa | ASTM D790 |
06 | Dart Drop (66 cm) | 90 g | ASTM D1709 |
07 | Tensile Strength at Yield, 50.8 mm/min MD | 24 MPa | ASTM D882 |
08 | Tensile Strength at Yield, 50.8 mm/min TD | 26 MPa | ASTM D882 |
09 | Elongation at Break, 50.8 mm/min MD | 480% | ASTM D882 |
10 | Elongation at Break, 50.8 mm/min TD | 640% | ASTM D882 |
11 | Elmendorf Tear Strength, MD | 19 g | ASTM D1922 |
12 | Elmendorf Tear Strength, TD | 270 g | ASTM D1922 |